Colour : Black /white /red/yellow/orange/blue
HDPE Sheet Thickness: 2-200 mm, 0.2-3 mm
HDPE Sheet Size: Length: 1220 mm, 1000×2000 mm
This kind of HDPE plastic sheet features more advance performance than standard HDPE sheeting. The enhanced highlights of HDPE pipe grade make it the most well-known HDPE sheet for open air applications.
Item | RESULT | UNIT | PARAMETER | NORM USED |
Mechanical properties | ||||
Modulus of elasticity | 1000 | MPa | In tension | DIN EN ISO 527-2 |
Modulus of elasticity | 1000 - 1400 | MPa | In flexure | DIN EN ISO 527-2 |
Tensile strength at yield | 25 | MPa | 50 mm/min | DIN EN ISO 527-2 |
Impact strength (Charpy) | 140 | Kj/m 2 | Max. 7,5j | |
Notched Impact stren. (Charpy) | No break | Kj/m 2 | Max. 7,5j | |
Ball indentation hardness | 50 | MPa | ISO 2039-1 | |
Creep rupture strength | 12,50 | MPa | After 1000 hours static load 1% elong. after 1000 hours Against steel p=0,05 N/mm 2 | |
Time yield limit | 3 | MPa | ||
Coefficient of friction | 0,29 | ------ | ||
Thermal properties | ||||
Glass transition temperature | -95 | °C | DIN 53765 | |
Crystalline melting point | 130 | °C | DIN 53765 | |
Service temperature | 90 | °C | Short term | |
Service temperature | 80 | °C | Long term | |
Thermal expansion | 13 - 15 | 10-5K-1 | DIN 53483 | |
Specific heat | 1,70 - 2,00 | J/(g+K) | ISO 22007-4:2008 | |
Thermal conductivity | 0,35 - 0,43 | W/(K+m) | ISO 22007-4:2008 | |
Heat distorsion temperature | 42 - 49 | °C | Method A | R75 |
Heat distorsion temperature | 70 - 85 | °C | Method B | R75 |